I've never tried or needed a silicate based product.
You really should try silicate based developer.
I have used NaOH for years, but now I don't want to touch it any more.
Silicate developer is way better, for 2 reasons :
1) HUGE margin between "Develop" and "strip", so you don't need to worry much about temperature, concentration and differences between laminates, you can use it really strong for quick 5-10 sec developing and still run minimal risk of stripping for up to a minute or so - this is also helpful if your UV box output isn't very uniform.
2) Solution has infiinite shelf-life - NaOH goes funny
*after a while - less of an issue if you make it up fresh, but if you have a permanent tank setup, with NaOH you need to drain & refill regularly. With silicate you just chuck some more in when dev times get longer.
* Excuse my lack of chemisty knowledge